Skip to content
Products
BRUTE Hydrazine
BRUTE Peroxide
Peroxidizer
Applications
Oxides
Nitrides
Resources
Technical Resources
ALD Oxide Wizard
ALD Nitride Wizard
Research Partners
About
About RASIRC
Our Team
News
Events
Sales Channels
Intellectual Property
Quality Assurance
Environment, Health and Safety
Supplier Relations
Careers
Contact
Products
BRUTE Hydrazine
BRUTE Peroxide
Peroxidizer
Applications
Oxides
Nitrides
Resources
Technical Resources
ALD Oxide Wizard
ALD Nitride Wizard
Research Partners
About
About RASIRC
Our Team
News
Events
Sales Channels
Intellectual Property
Quality Assurance
Environment, Health and Safety
Supplier Relations
Careers
Contact
Low Temperature Thermal Atomic Layer Deposition of Aluminum Nitride Using Hydrazine as the Nitrogen Source
Get full report
Products:
BRUTE Hydrazine
Applications:
ALD (Oxide/Nitride)
Films:
AlN
Back to all Resources
All Resources
June 2020
Get the Full Research Report
Fill out the form below to request the full PDF of this report.
Resource Request
Phone
This field is for validation purposes and should be left unchanged.
Name
(Required)
First
Last
Company Affiliation
(Required)
Email
(Required)
Scroll to Top